Share on:
Type | Style | Performance | ||||||||
Breaking Porce(N) | Elongation at break(%) | Diameter(MM) | Adhesion(N/CM) | Dry heat shrinkage(%) | ||||||
Polyester | 1100dt/*2 | ≥150 | 18.0±1.5 | 0.45±0.10 | ≥50 | ≤2.0 | ||||
1100dt/*3 | ≥190 | 18.0±1.5 | 0.45±0.10 | ≥60 | ≤2.0 | |||||
1440dt/*1 | ≥85 | 16.5±1.5 | 0.3±0.08 | ≥50 | ≤2.0 | |||||
1670dt/*1 | ≥100 | 11.0±1.5 | 0.35±0.10 | ≥50 | ≤3.0 | |||||
PVA | 1330dt/*1 | ≥90 | ≥8.5 | 0.3±0.05 | ≥50 | ≤1.5 | ||||
2000dt/*1 | ≥160 | 6.7±1.5 | 0.45±0.05 | ≥90 | ≤1.0 | |||||
2000dt/*2 | ≥350 | 6.7±1.5 | 0.65±0.05 | ≥120 | ≤1.0 | |||||
Rayon | 1840dt/*1 | ≥85 | ≥11.5 | 0.35±0.08 | ≥50 | - | ||||
Aramid | 1100dt/*1 | ≥200 | 3.3±1.0 | - | - | 1%:60±10N | ||||
1680/*1 | ≥300 | 3.5±1.0 | - | - | 1%:80±10N |