Share on:
1.Description
1)Excellent dot and isolated line reproduction
2)Solid printing performance
3)High latitude of exposure and processing
4)Good ink transfer
5)High impression
2.Technical parameters
Type | R394-II | R284H | R228-II | R170H | |
Thickness(mm) | 3.94mm | 2.84mm | 2.28mm | 1.70mm | |
Rigidity(Shore A) | 41-45 | 58-62 | 55-58 | 72-73 | |
Recommend relief depth(mm) | 1.8-2.0 | 1.0-1.4 | 1.0-1.2 | 0.7-0.9 | |
Image reproduction | 5%~95% | 2%~95% | 2%~95% | 2%~95% | |
Maximum line line/inch | 100 | 120 | 133 | 150 | |
Minimum isolated line | 0.3mm | 0.175mm | 0.15mm | 0.10mm | |
Minimum isolated dot | 0.50mm | 0.25mm | 0.20mm | 0.20mm | |
Suitable ink | Suitable for water and alcohol-based ink, incompatible with oil-based ink, hydrocarbon solvent or the ink containing ethyl acetate of more than 25% | ||||
Mainly applicable field | Corrugated board, thick board,paper | Label, flexible package, carry bag, folded paper box and beverage package | Label, flexible package, carry bag, folded paper box and beverage package | Film, Label, flexible package, carry bag, folded paper box and beverage package | |
Storage—raw plates | Unexposed plates should be stored in cool areas (4-32°C)away from heat. The plates must be placed flatly, and protected from contacting UV light. It is recommended to unpacked and handled in yellow light. | ||||
Storage—finished Plates | Printing plate should be avoid excessive white light, irradiating from sunlight and exposing in high concentrated ozone environments for a long time either. After being unloaded, the plates should be cleaned thoroughly. | ||||
Guarantee Period | Under the recommended storage condition, guarantee period of Flexographic Printing Plate is 12 months. | ||||
Packing | 60"*30"(1524mm*762mm), 8 pcs/ctn 40"*30"(1016mm*762mm), 8 pcs/ctn 42"*60"(1067mm*1524mm), 8 pcs/ctn | 80"*50"(2032mm*1270mm), 6 pcs/ctn | 80"*50"(2032mm*1278mm), 10 pcs/ctn |
3.Process parameters
Type | R394-II | R284H | R228-II | R170H |
Thickness( mm) | 3.94 | 2.84 | 2.28 | 1.70 |
Back exposure(seconds) | 35-70 | 25-40 | 35-55 | 15-21 |
Main exposure(minutes) | 8-20 | 8-20 | 8-20 | 10-18 |
Rinsing(minutes) | 5-7 | 5-7 | 5-7 | 5-7 |
Minimum drying time(hourrs) | 1.5-2 | 1.5-2 | 1.5-2 | 1.5-2 |
Detackfying(minutes)) | 5-7 | 8-15 | 5-7 | 5-8 |
Post exposure(minutes) | 3-5 | 5 | 5 | 5 |
4.Usage Scope
5.Packing
6.Processing
Suzhou Aolide Co., Ltd. was established in 2006, our company is engaged in the business offlexographic printing plates and Subliamtion transfer paper.
Suzhou Aolide Co.,Ltd is located in Suzhou city, Jiangsu Province, we enjoy convenient access to major transportation networks. Our company has around 50 staff members. Furthermore, all of our products are manufactured with advanced equipment and strict QC procedures in order to ensure high quality.
Please feel free to contact me online or send me a message if you are interested in our products, thank you!