Product Description


SE-805# & SE-810# silicone rubber is platinum cure silicone rubber (or called addition cure silicone rubber) based on medical grade certificated. It is two-components silicone rubber, it will be cured under room temperarure and can be cured fastly by heating. The product is colorless or skin-colored oily liquid and becomes soft elastic material after vulcanization.

 With platinum cured, it is environmental friendly, skin safe, odorless and nontoxic. Also, it have soft hardness and excellent tension and tear strength and resilience.





Characteristics:

- Medical grade, totally non-toxic, odorless, harmless, and eco-friendly
- Flesh tone color, skin color
- High elasticity; good tensile strength and tear strength
- Very suitable hardness
- Low shrinkage less than 0.1%
- Long service life of 5 years
- Good flexibility, permeability and easy operation
- Excellent UV-irradiation resistance and aging resistance



Model NO·
SE-800#
SE-805#
SE-810#
Mixing Ratio (by weight)
1:1
1:1
1:1
Appearance/Color
skin color
skin color
skin color
Hardness (Shore A)
0±2
5±2
10±2
Mixed viscosity (mPa·s)
1700±500
4000±500
1300±500
WorkingTime(at23℃/75℉,MINS)
30~40
30~40
30~40
Curing Time (at 23℃/75℉,HRS)
4~5
4~5
4~5
Tensile strength, Mpa
≥3.0
≥3.4
≥3.6
Tear strength, KN/m
≥5.4
≥12.7
≥14.8
Elongation at break, %
≥490
≥510
≥520


Applications:

The application would be used for making soft silicone rubber products like human body shape, breast pad making, bra pads, silicone breast and prosthesis, shoulder pads, patch, anti slip mat, anti-skid pad, silicone scar sheet, silicone dolls filling, bra filling, artificial vagina, etc.



Using instructions:

Step 1: Prepare and clean the prototype.
Step 2: Mixing part A and part B of our silicone rubber evenly according to the mixing ratio of 1:1 or 10:1.
Step 3: After mixed the silicone evenly, it is better to release the bubble by vacuum pumping.
Step 4: Pouring cast

Notes: Please finishes all the steps within the operation time. If not, it will cause cross linking reaction, and no more further steps will be available. So, we have to pay attention to the pot life and curing time.




Tin cure silicone comparison:

SEMOST silicone use imported raw material production , multi-layer filtration, fine and smooth, less bubbles, no impurities.
Inferior silicone use recycled material production, single filtration, many bubbles, with impurities.




Platinum cure silicone comparison:

SEMOST silicone use imported raw material production , multi-layer filtration, high transparency and good liquidity, less bubbles, no impurities.
Inferior silicone use recycled material production, single filtration, many bubbles,  with impurities.





Silicone mold performance comparison:

SEMOST silicone with super toughness, not easy to damage, high duplication times, clear copying pattern.

Inferior silicone with very low toughness, easy to damage, low duplication times, blurred copying pattern.



Detailed Image






Our Company


Guangdong SEMOST Biotechnology Co., Ltd. is a comprehensive technology enterprise specializing in the research, production, sales and service of organic liquid silicon collagen materials.

SEMOST are offering various kinds of liquid silicone in several industries. The products included 16 series in hundreds of kinds of silicone products like liquid silicone rubber, RTV-2 molding silicone rubber, condensation cure silicone rubber, addition cure silicone rubber, life casting silicone, silicone for medical application, food grade silicone rubber, silicone for fabric print, tyre mold silicone rubber, silicone gel, liquid foaming silicone, etc.





Our Goal:
Superior quality , Favorable price, Supreme service

SEMOST's collective mission is to design and manufacture the highest-performance line of liquid silicone rubbers and to provide our customers with unmatched, industry-setting technical support, favorable price and best customer service. In doing so, we believe it will help our customers for receiving the greatest value.



Our Service:
Customer first, Pursuit ideal, Serious and responsible, Win-win cooperation

Convenient and fast delivery, Experienced engineers, Long-term tracking of product performance monitoring and regular maintenance of after sales contact. Choose us, we will strive to provide safe and environmentally friendly raw material to you and contributing to your career.



Contact us:

Tel:+1-510-707-2906 
E-mail: [email protected]
Address: 632 Alice St, Oakland,CA 94607



Certifications






Packing & Delivery






FAQ



1.How to choose hardness for lifecasting silicone rubber?

When the life casting silicone rubber is applied to different parts of human, it requires different hardness.

To make the thin skin, the hardness is 20 to 25 shore A.

To make the breast, the hardness will be 5 shore A.

To make a complete finger, the hardness will be 8 to 10 shore A. If just to make a layer of skin, the hardness should be 20shore A.

To make the female sex toys, the silicone rubber must be very soft. For example, the silicone bra needs silicone with 3 to 5shore A, 0 shore A is required for especial.

To make the dildo, the hardness of inside should be 20shoreA,surface will be 0 shore A.

To make the vaginal or sex doll , the hardness should be less 0 shore A

To make the silicone mask, the hardness is 40 shore A.

To make the human model, which is filler inside and silicone outside, the hardness of silicone on the surface is 3 to 5 shore A.

To make the artificial limbs, the hardness will be 10 to 15 shore A.

Note: The special hardness should be confirmed with the customer and then recommend the suitable hardness.



2.Why does the silicone mold appear to dry outside but wet inside?
Some molding silicone rubber is a kind of condensation cure silicone rubber, which would get solidified after absorbing moisture. While in order to provide a significant shelf-life for the silicon rubber, we will dry out the water in the silicon rubber. So when the humidness is lower than 50%, this would happen.

Solution: Add 0.1% water into the silicon rubber and Stir over a low speed briefly when you use it. 




3.Why the silicone mould turns to be sticky?
The main reason for this problem is that we do not handle the products or original molds well.
We should deal with the mother mould carefully before molding. Such as for the products with a complicated
pattern or a unsmoothed surface, we should polish and clean the products, then spray the release agent. Normally, the release agent can be Vaseline, detergent. liquid wax Etc. In practical process, you can brush different release agent according to different material.

The second reason is that the operator pour the silicone into the mold when the mixture is not mixed evenly, so the finished silicone mold will not cured and dried entirely.