Сохранить в закладки:
PR | HP | UHP | ||
Electric Resistivity(μΩ·m) | ≤8.0 | ≤7.0 | ≤6.2 | |
Bending Strength(MPa) | ≥10.0 | ≥10.5 | ≥10.5 | |
Elestic modulus(GPa) | ≤12.0 | ≤12.0 | ≤14.0 | |
Bulk Density(g/cm3) | ≥1.66 | ≥1.62 | ≥1.58 | |
Coefficient of Thermal Expansion(X10-6/℃) | ≤2.7 | ≤2.4 | ≤1.5 | |
Ash(%) | ≤0.3 | ≤0.3 | ≤0.3 |