Copper Cathode and Pure Copper Ingot 99.99%

Share on (10000007828057):


Price:

Quantity:


Product Overview

Description














































Material


CuBe


Material no. UNS (ASTM)


C17200 C17500 C17510


Material description


Hardenable Cu-alloy with high electrical and thermal conductivity with

a high degree of hardness and strength. 


Standard


R.W.M.A Class 3


Hardness


220-280 HB 10/2,5


Thermal conductivity


20℃ ca. env. 240 W/m.K, 300℃ env. 260 W/m.K


Electrical conductivity


min. 25, min. 45% IACS MS/m


Softening temperature 


480℃


Size


According to customer's requirements


Application


Electrical contact


 


 


7553 (1).jpg7553 (1).png7553 (2).jpg7553 (3).jpg7553 (4).jpg


 


 


 


 


 


 