Share on:
Part of the Parameters of the WS Dissolvable Rubber Cylinder | Item | Data | ||||||
Type | Temperature /Celsius | Hardness /Shore A/GB/T531 | Tensile strength/Mp/GB/T128 | Complete degradation tim(13*32mmcylinder) | ||||
WS30 | 20-40 | 75-85 | >12 | within 150h in 30 degrees | ||||
WS40 | 30-50 | 75-85 | >12 | within 150h in 40 degrees | ||||
WS50 | 40-60 | 80-90 | >18 | within 120h in 50 degrees | ||||
WS60-1 | 50-70 | 80-90 | >18 | within 120h in 60 degrees | ||||
WS60-2 | 50-70 | 75-85 | >18 | within 120h in 60 degrees | ||||
WS70 | 60-80 | 80-90 | >18 | within 120h in 70 degrees | ||||
WS70k | 60-80 | 80-90 | >18 | within 120h in 70 degrees | ||||
WS90 | 90-110 | 80-90 | >17 | within 150h in 90 degrees | ||||
WS90-4 | 80-110 | 80-90 | >18 | within 150h in 90 degrees | ||||
WS90-5 | 80-110 | 75-85 | >18 | within 150h in 90 degrees | ||||
WS130 | 110-130 | 80-90 | >18 | within 240h in 90 degrees | ||||
WS140 | 130-150 | 80-90 | >18 | within 240h in 90 degrees |