Grade



Density 


g/cm3



Shore Hardness



Apparent porosity   %



compression strength 


Mpa



Flexural Strength  Mpa



M106H



1.65



60



2



125



51



M258



1.9



50



2



88



42



EK60



1.74



105



1



 



75



V1626



1.85



90



10



150



58



 


 


 


 


 


 



Product Description


 




2. About our company  : 


 


1. we supply all various kinds of graphite plate of vacuum pump,it was stable with high temperature and have a strong resistance to chemical corrosion


 


2. we can give your a discount when get your bulk order,different specification have different price 


 


3. have our independent factory and reasonable price superior quality,first-class material and different service 


 


 



3.  About products : 


 


1.  non-standard graphite sheet or graphite blade can be design as per your samples or drawing


 


2. on the other hand,it has a strong function of lubrication


 


3.  it was comprehensive performance to meet customer's requirement.


 


 


 


 


 


 



Detailed Images


DSC00949


 


DSC01432


 


DSC00949




 2 (1)_.jpg2 (6)_.jpg


 



Packaging


Packing & Delivery__.jpg 





FAQ


1. Why choose us ? 



  • Technical support  - Technical people have experience in this period over 35 years.




  •  Material support   - carbon graphite, soft graphite, electrographitic , impregnated graphite , 

                                              Resin grapihte,  metal graphite,  impreganated metal graphite , 


                                               Natural grpahite ,  Resin bonded .


       


  • Producing support  - Using professinal machines and technological guidance .   


     





 


2.Can we use our design ? 
Yes, you can. After getting your detial design drawings , we do same .


 


 


 


 


 


 


3. Can we mix the different design products ? 
Yes, you can modify.


 


 


 


 


 


 


 


4.  Failure cause ?


















































Technical hitches 



Causation



Repair



 


 


Brush spark 



1.Commutator deformed 



1.Loosen the fastening screws to re-adjust



2. Copper barbed or sharp edges



2. Re-chamfer



3. Brush pressure is too small



3. Adjust or replace the spring pressure



    Brush overheating



1. Brush too much pressure



1. Adjust or replace the spring pressure



2. Single Brush pressure imbalance



2. Replacing different carbon brushes



 


 


Wear fast




  1. 1. Commutator was dirty



1. Clean commutator



2. Copper barbed or sharp edges obvious



2. Re-chamfer



3. Load is too small to form an oxide film



3. Improve load or minus number of brushes



 


4.Work environment is too dry or too wet



4.Improve the working environment or replacement brush card



 


 





0.1929 s.