Composition | By alkyd resin, petroleum asphalt liquid pigment after grinding, adding additives and organic solvent modulation. | ||||
Application | Used for waterproof and anticorrosive coating of indoor and outdoor steel surfaces and buildings and pipes with anticorrosive primer. | ||||
Basic parameters | Wet film thickness 70-85um | Dry film thickness 30-35um | 0.13-0.25 kg/㎠ theoretical dosage | ||
Drying time:Surface dry 24H / Overall dry 72H | |||||
Resistance to impact 50cm | |||||
No abnormal heat resistance for 120 hours | |||||
No abnormal salt mist tolerance for 120 hours | |||||
Water resistance 30d no abnormal | |||||
Salt resistant water (immersed in 3% NaCl solution for 72 hours) no abnormal | |||||
Acid resistance (Immersed in 5% H2SO4,dissolvability,for 72 hours)No abnormality | |||||
Volatile oil resistance (immersed in No .3 ordinary paint and solvent oil for cleaning for 48 hours) no abnormal | |||||
Bending test | 10mm | ||||
Recommended number of painting routes | 2 | ||||
Repainting interval | Not less than 24h | ||||
Base temperature | above 3 ℃ Celsius above dew point | ||||
Coating method | air spraying, airless spraying, brush coating | ||||
Mix ratio | Main paint : Diluent =1:0.5(weight ratio) | ||||