Share on (1600259948643):
CoreClad Concentricity, μm | ≤ 0,80 |
Cladding Diameter, μm | 125±0,7 |
Cladding NonCircularity, % | ≤ 2,0 |
Coating Diameter, μm | 243,5±3,0 |
Fiber Curl, m radius of curvature | ≥ 4 |
CoatingCladding Concentricity, μm | ≤ 12 |
Length*, km | 25,2 / 50,4 |
Maximum Attenuation*, dB/km at wavelengths | ||
1550 nm | ≤ 0,17 | |
1625 nm | ≤ 0,19 | |
Attenuation vs. wavelength | ||
1285-1330 nm at wavelength 1310 nm | ≤ 0,02 | |
1525-1575 nm at wavelength 1550 nm | ≤ 0,03 | |
Point discontinuity, dB | ||
1550 nm | ≤ 0,05 | |
Mode Field Diameter, μm | ||
1550 nm | 11,5±0,7 | |
Cable Cutoff wavelength, (λсс ), nm | ≤ 1530 | |
Dispersion, ps/nm·km | ||
1550 nm | ≤ 22 | |
1625 nm | ≤ 28 | |
Dispersion slope at 1550 nm, ps/nm2·km | So≤ 0,070 | |
Polarization Mode Dispersion (PMD), ps/√k | FA2 | |
Maximum Individual Fiber PMD | ≤ 0,1 | |
PMD Link Design Value | ≤ 0,06 | |
Proof Test, GPa | ≥ 0,69 | |
(Other tension force on request) % | >1% | |
Coating Strip Force, N | ||
Peak force | 1 – 8,9 | |
Typical average force | 1 – 5 | |
Dynamic Stress Corrosion Susceptibility Parameter (Nd) | ≥ 20 | |
Induced Attenuation 1310 nm, 1550 nm & 1625 nm, dB/km | ||
60ºC ~ +85ºC Temperature dependence | ≤ 0,05 | |
+23ºC Water Immersion | ≤ 0,05 | |
+85ºC Heat Aging | ≤ 0,05 | |
+85ºC/85%Damp Heat | ≤ 0,05 | |
Effective Group Index of Refraction | ||
1550 nm | 1,464 | |