Principle·Parameter·Technical Description
A series of operations such as vacuum, pressure, and heating are used, and then the corresponding concentration of anti-corrosion, flame-retardant, and dyeing liquids are injected into the wood cells through vacuum, high pressure, and frequency pressure to achieve anti-corrosion, moth-proof, termite-proof, and flame-retardant And dyeing and other effects.
Principle·Parameter·Technical Description
1 Equipment pressure: 01~4.0MPA 2 Vacuum degree: 0~-0.098MPA 3 Design temperature: 0~180 degrees Celsius
4 Working medium: water-soluble anti-corrosion, flame retardant, dyeing agent 5 years output: 5000 cubic meters to 20000 cubic meters
Principle·Parameter·Technical Description
Quick opening method: manual quick opening
2) Sealing method: inflatable silicone seal
Ring, the sealing effect is obviously better than other methods, the service life is more than 1 year
3) Safety interlock mode: ①Pressure automatic safety
Interlock ②Manual safety interlock
Control method: adopt electrical automatic control, PLC computer automatic control, manual control. Additional execution methods: indirect steam heating, guided oil heating, electric heating, direct steam heating 6) Vacuum method: vacuum pump automatically controls the tank
The degree of vacuum.
Pressurization method: the high-pressure pump automatically pressurizes the tank and stops automatically when the pressure reaches the pressure, and automatically pressurizes when the pressure is lower than the pressure.
8
Time mode: When the set working time is reached, the power will be automatically cut off and the alarm will be triggered. AN TAI
Principle·Parameter·Technical Description
A series of operations such as vacuum, pressure, and heating are used, and then the corresponding concentration of anti-corrosion, flame-retardant, and dyeing liquids are injected into the wood cells through vacuum, high pressure, and frequency pressure to achieve anti-corrosion, moth-proof, termite-proof, and flame-retardant And dyeing and other effects.
Principle·Parameter·Technical Description
1 Equipment pressure: 01~4.0MPA 2 Vacuum degree: 0~-0.098MPA 3 Design temperature: 0~180 degrees Celsius
4 Working medium: water-soluble anti-corrosion, flame retardant, dyeing agent 5 years output: 5000 cubic meters to 20000 cubic meters
Principle·Parameter·Technical Description
Quick opening method: manual quick opening
2) Sealing method: inflatable silicone seal
Ring, the sealing effect is obviously better than other methods, the service life is more than 1 year
3) Safety interlock mode: ①Pressure automatic safety
Interlock ②Manual safety interlock
Control method: adopt electrical automatic control, PLC computer automatic control, manual control. Additional execution methods: indirect steam heating, guided oil heating, electric heating, direct steam heating 6) Vacuum method: vacuum pump automatically controls the tank
The degree of vacuum.
Pressurization method: the high-pressure pump automatically pressurizes the tank and stops automatically when the pressure reaches the pressure, and automatically pressurizes when the pressure is lower than the pressure.
8