Share on (1600424611734):
Wholesale Customized Thermal Conductive Silicone Insulation Pad
3


Physics parameter form
| Test Item | Test Method | Unit | CP800 Value |
Color | Visual |
| Blue |
Thickness | ASTM D374 | mm | 0.5-5mm |
Specific Gravity | ASTM D792 | g/cc | 3.5±0.1 |
Hardness | ASTM D2240 | Shore C | 25±5 |
Tensile Strength | ASTM D412 | (Pa) | 5.88*108 |
Compressibility | ASTM D412 | % | 30 |
Temperature Range | EN344 | ℃ | -40~+150 |
Volume Resistivity | ASTM D257 | Ω-CM | 1.0*1011 |
Breakdown Voltage | ASTM D149 | KV/mm | 4 |
Flame Rating | -94 |
| V-0 |
Thermal Conductivity | ASTM D5470 | w/m-k | 8.0 |


Product Pictures:



Application mode:
1. Fill between the circuit board and thermal slug
2. Fill between IC and thermal slug or the product shell
3. Fill between IC and heat dissipation material ( such as metallic shield)
Product application:
Thermal silicone pad is widely used for all kinds of high power supply, laptop, LED light, smartphone, power battery, electronic industry and so on.
Certifications:

Factory show:




A: We are manufacturer, our factory in Dongguan city, China. Welcome to visit.
A: Generally it is 5-7 days if the goods are in stock. or it is 15-20 days if the goods are not in stock, it is according to quantity.
A: Yes, we could offer the sample for free , but not including the shipping cost.
A:If you are ordering a unique sample that we don't have in stock, you need to provide all the details, it will be better if you can send a sample for our evaluation. Customized samples maybe need new molding, which will cost molding fee. We will check your sampling requirements, then issue a sampling P/I. Sampling may take 3-5 days, depending on detailed samples.
Any more questions, please contact us freely.
PS:If you want to know more about our product, pls feel free to contact us. And welcome to our factory.

New products from manufacturers at wholesale prices