1.4x1.4x1.6mm n p type bismuth telluride bi2te3 pellet bismuth telluride thermoelectric element
Characteristics: | Bismuth telluride is a compound of tellurium and bismuth. It is a narrow gap layered semiconductor with a trigonal unit cell. It mainly occurs in a rare mineral tellurobismuthite. It's produced by sealing bismuth and tellurium metals in a quartz tube under vacuum. When alloyed with selenium or antimony, it acts as an efficient thermoelectric material suitable for portable power generation or refrigeration. |
Production Processes: | Vacuum melting - crystallization (crystal orientation growth) - regional melting - removal of both ends; |
Applications: | Forming P/N section for semiconductor refrigeration, thermoelectric power generation, etc. |
2.General Properties
Place of Origin | Hubei,China |
Brand Name | Tuocai |
Material | bismuth, tellurium, selenium, antimony |
Chemical Composition | 99.99% 4n |
Molecular formula | Bi2Te3, Bite |
CAS No. | 1304-82-1 |
Density | 7.73g/cm3 |
Melting point | 586℃ |
Surface | With Ni & Sn Plated |
Doping | P type bismuth telluride doped Antimony N type bismuth telluride doped Selenium |
Seebeck (S) | 210-230 (alpha, μ V / k) at 300K |
Electrical conductivity | 950-1050 (alpha, μ V / k) at 300K |
![]() | Product Model: | N-type semiconductor components |
Production Process: | Zone melting crystal pulling process with coating | |
Purity: | 99.99% | |
Size: | 1.4x1.4x1.6mm(L*W*H) Also can be customised on request | |
Seebeck coefficient: | 205-210 (α, μ V / k) at 300K | |
Electrical resistivity: | 1.0 (ρ u Ω. Cm) at 300K | |
Electrical conductivity: | 950-1050 (α, μ V / k) at 300K |
![]() | Product Model: | P-type semiconductor components |
Production Process: | Powder metallurgy with coating | |
Purity: | 99.99% | |
Size: | 1.4x1.4x1.6mm(L*W*H) can be customised on request | |
Seebeck coefficient: | 205-210 (α, μ V / k) at 300K | |
Electrical resistivity: | 1.0 (ρ u Ω. Cm) at 300K | |
Electrical Conductivity: | 950-1050 (σ, S / cm) at 300K |
| Bismuth Telluride Powder: | gneral particle size is 120 mesh,200/325/500/1250mesh are also available. |
| Bismuth Telluride Pellet: | gerneral size is 1.4x1.4x1.6mm,other size can be customised. |
| Bismuth Telluride Wafer: | size as per your requirements. |
| Bismuth Telluride Rod: | general size of n type round rod is 28mm diameter x 150mm height, p type square rod is 30mm length x 30mm width x 100mm . |


Product Name: | 1.4x1.4x1.6mm n p type bismuth telluride bi2te3 pellet bismuth telluride thermoelectric element |
Package: | N-type and P-type pellets are separately packed in vacuum storage bag or as per your requests. |
Shipping Way: | By Air, Sea, Couriers like FedEx, UPS, DHL etc. |
Delivery Time: | It generally takes roughly 5 workdays after order confirmed.Depends on your order. |






New products from manufacturers at wholesale prices