sapphire wafers are made of sapphire/ruby ,they are widely applied to medicine, accurate machine, accurate measure and inspection and laser technology. They also contribute a lot in the anticorrosion, wearable and high heat conduction environments.
synthetic sapphire blank, cup bearing, stick, balls, windows, and other special parts according to customer's drawings or request.
MAN MADE CORUNDUM PROPERTY | ||||
General | Chemical Formula | Al2O3 | ||
Crystal System | Trigonal | |||
Class | Hexagonal-scalenohedral | |||
Melting Temperature | 2030°c | |||
Thermal | Thermal Expansion | Parallel to C-axis: 6.7× 10-6 | ||
Perpendicular to C-axis: 5.0×10-6 | ||||
Specific Heat | 0.18 Cal/gmoK(25℃) | |||
Mechanical | Density | 3.98 ~ 4.1g/cm3 | ||
Hardness | 9Moh’s Scale | |||
(Hv)≥1700kg/mm2 | ||||
Modulus Of Elasticity | 340-380Gpa | |||
Compressive Strength | 2.1Gpa | |||
Tensile Strength | 0.19Gpa | |||
Optical | Index of Refraction | Parallel to C-axis:1.769 | ||
Perpendicular to C-axis:1.76 | ||||
Index of IR Transmission | 85% | |||
Electrical | Electrical Resistance | 1016 Ω/cm(25°c) | ||
Dielectric Constant | 7.5-10 | |||
Chemical | Corrosion Resistance | Can not be corroded by acid or alkali at normal temperature, only can be corroded by HF at 300°c | ||