Property | Unit | Value | Method | |||
Density | g/cm3 | ≥ 0.90 | GB/T 22308-2008 | |||
Tensile Strength,AMD | MPa | ≥ 5.5 | GB/T 20671.7-2006 | |||
Compressibility | % | 25.0~45.0 | GB/T 20671.2-2006 | |||
Recovery | % | ≥ 15.0 | ||||
Fluid Resistance, IRM 903 Oil(150℃,5h) | ||||||
Change in weight | % | ≤ 55.0 | GB/T 20671.3-2006 | |||
Change in thickness | % | ≤ 10.0 | ||||
Change in compressibility | % | ≤ 45.0 | ||||
Notes:Specification values are determined by the test methods required for GB/T20671.1-2006, Type 7 materials. |