Physical properties of | Test conditions | The test method | The test data | The data unit |
The proportion of | / | ISO 1183 | 1.13 | g/cm3 |
Melt flow rate | Melt flow rate | ASTM D1238 | 27 | g/10 min |
shrinkage | Flow: 1.60mm | ASTM D955 | 0.12-0.18 | % |
Bibulous rate | 23°C, 24 hr | ISO 62 | 0.060 | % |
Rockwell hardness | M meter scale | ASTM D785 | 87 | / |
Mechanical properties of | ||||
Tensile stress | yield | ISO 527-2 | 55.0 | MPa |
Tensile strain | The fracture | ISO 527-2 | >120 | % |
Bending modulus | / | ISO 178 | 2450 | MPa |
The bending strength | / | ISO 178 | 83.0 | MPa |
Thermal performance | ||||
Thermal deformation temperature | 0.45mpa, unannealed | ISO 75-2/B | 155 | °C |
1.8 MPa, without annealing | ASTM D648 | 60.0 | °C | |
The melting temperature | / | DSC | 223-227 | °C |
Linear expansion coefficient | The flow | ASTM D696 | 0.000090 | cm/cm/°C |
Electrical properties | ||||
Surface resistivity | / | IEC 60093 | 1.0E+13 | ohms |
Volume resistivity | / | IEC 60093 | 1.0E+15 | ohm.cm |
Dielectric strength | 2.00mm | ASTM D149 | 20 | V/mm |
Dielectric constant | / | ASTM D150 | ASTM D150 | / |
Dissipation factor | / | ASTM D150 | 0.0010 | / |
The electric arc resistance | / | ASTM D495 | 120 | sec |
UL flame retardant rating | 3.20mm | UL 94 | HB | / |