Share on (1600618484038):


Physical properties of Taiwan ChiMei ABS- PA 777E | The test conditions | The test method | The test results | unit | |
Density/specific gravity | ASTM D-792 | 1.07 | 23/23 ℃ | ||
Melt index | 220 ℃ x 10 kg | ISO-1133 | 5 | g/10min | |
Mechanical properties of | The test conditions | The test method | The test results | unit | |
The tensile strength | ASTM D638/ISO 527 | 460 (6,530) | Kg/cm squared (MPa) Lb/in squared | ||
Rockwell hardness | ASTM D-785 | 115 | R | ||
ASTM D785 | R-115 | ||||
elongation | ASTM D638/ISO 527 | 10 | % | ||
Elasticity at bending | ASTM D-790 | 2.5 x 104 | kg/cm2 | ||
ASTM D-790 | 3.5 x 105 | lb/in2 | |||
Bending modulus | ASTM D790/ISO 178 | 23000 (32000). | Kg/cm squared (MPa) Lb/in squared | ||
The bending strength | ASTM D790/ISO 178 | 700 (9,900) | Kg/cm squared (MPa) Lb/in squared | ||
ASTM D-790 | 10630 | lb/in2 | |||
ASTM D-790 | 750 | kg/cm2 | |||
Extension and strength | ASTM D-638 | 6240 | lb/in2 | ||
ASTM D-638 | 440 | kg/cm2 | |||
IZOD notched impact strength | ASTM D256/ISO 179 | 12 (2.2) | Kg, cm/cm (J/M) ft lb/in | ||
ASTM D256/ISO 179 | 11 (2.0) | Kg, cm/cm (J/M) ft lb/in | |||
IZOD impact strength | 1/8" | ASTM D-256 | 12 | kg.cm/cm | |
1/4" | ASTM D-256 | 11 | kg.cm/cm | ||
1/4" | ASTM D-256 | 2 | ft.lb/in | ||
1/8" | ASTM D-256 | 2.2 | ft.lb/in | ||
Thermal performance | The test conditions | The test method | The test results | unit | |
combustibility | File No. E56070 UL&C-UL | 1/16"HB | |||
Combustibility (rate) | UL94 | 1.6 mmHB | |||
Thermal deformation temperature | ASTM D648/ISO 75 | 120 (248). | ℃ (℉) | ||
ASTM D648/ISO 75 | 109 (228). | ℃ (℉) | |||
ASTM D-648 | 109 (228). | ℉ | |||
ASTM D-648 | 120 (248). | ℃ | |||
Vica soften it up | ASTM D-1525 | 129 | ℃ | ||
ASTM D1525/ISO R306 | 129 (264). | ℃ (℉) | |||
ASTM D-1525 | 264 | ℉ | |||
Processing performance | The test conditions | The test method | The test results | unit | |
Dry conditions | Bake at 100~110°C for about 3 hours | ||||
The processing temperature | 220 ~ 250 ℃ | ℃ | |||
240 ~ 270 ℃ | ℃ | ||||
220 ~ 270 ° C | ℃ | ||||
Mold temperature | 40 ~ 80 ° C | ℃ | |||
pressure | 40 ~ 60 kg/cm squared | Mpa | |||
5 ~ 15 kg/cm squared | Mpa | ||||
50-70 kg/cm squared | Mpa | ||||
Physical performance | The test conditions | The test method | The test results | unit | |
Specific gravity (density) | ASTM D792/ISO 1183 | 1.07 | |||
Melt index (flow coefficient) | ASTM D1238/ISO 1133 | 4 | g/10min | ||