Product | Type | 25℃ pa.s Viscosity | Min Gel Time | Non -volatile | MPa Tensile Strength | Elongation | MPa Flexural Strength | HDT ℃ | ||||
SWANCOR 901 | General purpose | 0.35-0.55 | 15.0-25.0 | 54.0-56.0 | 90-95 | 5.5 | 130 | 101 | ||||
SWANCOR 907 | High performance phenolic epoxy Vinyl resin | 0.28-0.58 | 15-25 | 62±1% | 76-90 | 4 | 145 | 150 | ||||
SWANCOR 977-S | High temperature, solvent resistant type Vinyl resin | 0.6-0.9 | 25-35 | 73.5-69.5 | 62-80 | 2.5 | 125 | 210 | ||||
SWANCOR 907-S | High temperature resistant type Vinyl resin | 0.27-0.4 | 15-25 | 67±1% | 76-90 | 3.7 | 145 | 150 | ||||
SWANCOR 900 | High temperature, strong corrosion modified phenolic epoxy vinyl ester resin | 0.25-0.45 | 20.0-30.0 | 63.5-65.5 | 75-85 | 2.5 | 125 | 170 | ||||
SWANCOR 915 | Flame-resistant vinyl ester resin | 0.25-0.45 | 15±5min | 55±1% | 75-85 | 7 | 135 | 93 | ||||
SWANCOR 901-200 | Vacuum infusion process low viscosity vinyl ester resin | 0.15-0.25 | 10-125 | 55±1% | 76-90 | 5.5 | 135 | 102 | ||||
901-200P | 0.15-0.25 | 10-125 | 55±1% | 76-90 | 5.5 | 135 | 102 | |||||
901-200T | 0.25-0.45 | 10-125 | 55±1% | 76-90 | 5.5 | 135 | 102 | |||||
901-200PT | 0.25-0.45 | 10-125 | 55±1% | 76-90 | 5.5 | 135 | 102 | |||||
SWANCOR CP95 | Special primer resin for concrete lining projects | 0.10-0.30 | 5.0-15.0 | |||||||||
SWANCOR 901-PW | Vinyl ester resin primer paint | 0.5-0.7 | 10.0-20.0 | |||||||||
SWANCOR 983-M | Pre-accelerated iron base coated with vinyl ester resin | 20-30 | ||||||||||
SWANCOR 901-TPW-7X | Medium temperature pre-accelerated vinyl resin chrome green topcoat | 0.5-0.7 | 10-20 | |||||||||
SWANCOR 901-PW-6X | Medium temperature pre-accelerated Vinyl resin mouse gray finish | 0.5-0.7 | 10-20 | |||||||||
SWANCOR901-FLTP-7X | Trowel coated glass flake vinyl resin | 40-60 | >25 | >65 | 120 | |||||||


Appearance | 1. Brown and clear liquid |
Density | 2. 1.04±0.01 |
Viscosity | 3. 450±100cps(LVT#3-60rpm/25℃) |
Solid content | 4. 55±1% kg/L |
Gel time | 5. 15-25 min 6. (55%MEKPO:1.2%,6% cobalt octoate :0.4%,100%DMA: 0.05%,temperature:25℃ water bath) |
Storage period | 7. 9 month(below 25℃) |
Tensile strength | 8. 76-97 MPa | 9. (ASTM D 638) |
Tensile modulus | 10. 3.3-3.6 GPa | 11. (ASTM D 638) |
Elongation | 12. 5.0-6.0% | 13. (ASTM D 638) |
Bending strength | 14. 115-138 MPa | 15. (ASTM D 790) |
Bending modulus | 16. 3.1-3.4 GPa | 17. (ASTM D 790) |
Distortion temperature | 18. 100-102℃ | 19. (ASTM D 648) |
Hardness | 20. 30-38Barcol | 21. (ASTM D 2583) |
Temperature | Curing system | 10~20 minutes | 20~40 minutes | 40~60 minutes |
5~10℃ | 55%MEKPO | 3.0% | 3.0% | 3.0% |
5~10℃ | 2% cobalt | 2.4% | 1.8% | 1.8% |
5~10℃ | 100%DMA | 0.15% | 0.1% | 0.06% |
10~20℃ | 55%MEKPO | 1.5% | 1.5% | 1.5% |
10~20℃ | 2% cobalt | 2.4% | 2.4% | 1.2% |
10~20℃ | 100%DMA | 0.08% | 0.05% | 0.05% |
20~28℃ | 55%MEKPO | 1.2% | 1.2% | 1.2% |
20~28℃ | 2% cobalt | 1.2% | 1.2% | 1.2% |
20~28℃ | 100%DMA | 0.07% | 0.05% | 0.01% |
28℃ above | 55%MEKPO | 1.2% | 1.2% | 1.2% |
28℃ above | 2% cobalt | 1.5% | 1.2% | 0.9% |
28℃ above | 100%DMA | 0.06% | 0.04% | 0 |