1.The color materials are all powdered and need to be prepared by themselves. 2.The pigment will precipitate and separate for along timeand due to the different proportion of each pigment, the proportion ot Glaze Water Different, it is normal to deposit or agglomerate for a long time, stirring evenly and sieving Just use it. 3The pictureshows fiaure photo ofthe dry piament and the firina effect of alaze on white porcelain clav.
Asaresult, the color will be diflerent from that of Glaze Water
4.The firing effect ofqlaze is related to the temperature, heating curve, work shape, placement position and glazingthickness of kiln firingThecolor materials fired in different batches will also have slight differences.
There is no quarantee that the same effect can be burnt out in the details of this store. Please also conduc
samples before mass production for batch replacement. We hope to know it.
5.The glaze formula will be updated occasionally. Please confirm with the customer service before purchasing. The de ailed pictures in the store will be updated in time. Please refer to the effect of the color plate on the picture