Share on (1600829011948):
ExxonMobil HDPE HMA016 | ||||||
Physical property | Standard | Value | Unit | |||
Density | ASTM D1505 | 0.956 | g/cm³ | |||
Melt Index 190°C 2.16kg | ASTM D1238 | 20 | g/10min | |||
Environmental Stress Crack Resistance 10%lgepal 50°C | ASTM D 1693 | 2 | hr | |||
Mechanical behavior | Standard | Value | Unit | |||
Tensile Strength Yield | ISO 527 | 23 | MPa | |||
Elongation Yield | ISO 527 | 10 | % | |||
Elongation Break | ISO 527 | 100 | % | |||
Flexural Modulus | ISO 178 | 970 | Mpa | |||
Izod Notch Impact | ISO 180 | 4.0 | kJ/m2 | |||
Thermal | Standard | Value | Unit | |||
HDT 0.45MPa | ISO 75 | 64 | °C | |||
Melting Temperature Peak | ASTM D3418 | 133 | °C | |||










Product name | Hdpe virgin granules |
Color | Transparent, white, black, bule or customized |
Processing level | Extrusion grade. Injection grade. |
Use | Home appliances, office desks and chairs, sports equipment, auto parts Luggage accessories, kitchen knives, trash cans, manhole covers, water pipe elbows, etc |
Feature | Good wear resistance, electrical insulation, toughness and cold resistance; Good chemical stability |