Share on (1600901797511):







Number | Project | Unit | H40S | Test value | Test Methods | ||||||
1 | Melt mass-flow rate(MFR) | Nominal value | g/10min | 37 | 37.3 | GB/T 3862 | |||||
Deviation | ±37 | ||||||||||
2 | Isotactic index | % | >=96.0 | 97.51 | GB/T 2412 | ||||||
3 | Particle appearance | Color grain | Pc/kg | <=5 | 0 | SH/T 1541-2006 | |||||
Black grain | Pc/kg | 0 | 0 | ||||||||
Large and small grains | g/kg | <=100 | 0.1 | ||||||||
Snake skin grains and trailing grains | Pc/kg | report | 25 | ||||||||
4 | Impurities and others | Pc/kg | no | no | SH/T 1541-2006 | ||||||
5 | Ash | % | <=0.030 | 0.014 | GB/T 9345.1 | ||||||
6 | Tensile properties | Tensile modulus of elasticity(Et) | MPa | >=1200 | 1250 | GB/T 1040 | |||||
Tensile yield stress(σ y) | MPa | >=30.0 | 30.9 | ||||||||
Tensile stress atbreak(σ B) | MPa | >=8.0 | 20.7 | ||||||||
Nominal tensile strain at break(ε tB) | % | >=200 | 566 | ||||||||
Test conclusion | Qualified | ||||||||||






New products from manufacturers at wholesale prices