MICC Resistance wire used at operating temperatures up to 1200 degrees NiCr8020, NiCr7030 NiCr6015, NiCr3520 Types available

Share on (1600939229704):


Price:$25.00 - $35.00

Quantity:


Product Overview

Description


Resistance wire used at operating temperatures up to 1200 degrees NiCr8020, NiCr7030 NiCr6015, NiCr3520 Types available Cr20Ni80-3.JPG

 

Resistance wire(heating wire) used at operating temperatures up to 1200. Its chemical composition gives
 good oxidation resistance especially under conditions of frequent switching or wide temperature fluctuations.

 

 Applications include heating elements in both domestic and industrial appliances and in control resistors.
 Ni-Cr materials are widely used in industrial electric furnaces, household appliances and far-infrared devices
 because of their high temperature strength and strong plasticity.





















































































































Main property of NiCr  electric heating alloy
property typeCr20Ni80Cr30Ni70Cr15Ni60Cr20Ni35Cr20Ni30
Main chemical
composition%
NiRestRest55~6134~3730~34
Cr20~2328~3115~1818~2118~21
Fe  RestRestRest
Max continuous
 Temp.of element(℃)
12001200115011001100
resistivity(mm²/m)1.091.091.1211.04
Density((g/cm³))8.48.48.27.97.9
Thermal conductivity(KJ/M.h℃)60.360.345.243.843.8
Coefficient of liner
expansion(a*10-5/℃)
1818171919
Melting point (℃)14001400139013901390
Elongation(%)720720720720720
Micrographic structureAusteniticAusteniticAusteniticAusteniticAustenitic
Magnetic propertyNONENONENONENONENONE

 


 


   Main characteristics of Ni-Cr electric heating alloys
 























































































































  Alloy Nomenclature/Performance         Cr20Ni80         Cr30Ni70         Cr15Ni60         Cr20Ni35         Cr20Ni30
         Main
         Chemical
          composition
         Ni         Rest         Rest         55.0-61.0         34.0-37.0         30.0-34.0
         Cr         20.0-23.0         28.0-31.0         15.0-18.0         18.0-21.0         18.0-21.0
         Fe         ≤1.0         ≤1.0         Rest         Rest         Rest
         Max. continuous service temp. of element                  1200         1250         1150         1100         1100
         Resistivity at 20°C(μΩ·m)                  1.09         1.18         1.12         1         1.04
         Density (g/cm3)                  8.4         8.1         8.2         7.9         7.9
         Thermal conductivity(KJ/m·h·°C)                  60.3         45.2         45.2         43.8         43.8
         Coefficient of lines expansion(α×10-6/°C)                  18         17         17         19         19
         Melting point (approx.)( °C)                  1400         1380         1390         1390         1390
         Elongation at rupture (%)                  >20         >20         >20         >20         >20
         Micrographic structure                  austenite         austenite         austenite         austenite         austenite
         Magnetic properties                  nonmagnetic         nonmagnetic         nonmagnetic         Weak magnetic         Weak magnetic