Share on (1601001360077):




project | Test standard | Unit | SX-306 | ||
ISO | |||||
optical properties | Refractive index | ISO 489 | 1.49 | ||
Transmittance | ISO 13468-1 | % | >93 | ||
Fuzzy coefficient(Haze) | ISO 14782 | % | 0.3 | ||
Thermodynamic properties | Coefficient of linear expansion | ISO 11359-2 | 1/C | 7x10-5 | |
Vicat softening temperature(VST) | ISO 306 | °C | >101 | ||
1.82MPaLoad thermal deformation temperature | ISO 75-2 | °C | 94 | ||
230°C3.8kgMelt flow coefficient | ISO 1133 | g/10min | 1.6 | ||
Mechanical properties | tensile strength | ISO 527-2 | MPa | 74 | |
Tensile rate | ISO 527-2 | % | 6 | ||
Flexural strength | ISO 178 | MPa | 125 | ||
Flexural modulus | ISO 178 | MPa | 3300 | ||
CharpyImpact strength (with notch) | ISO 179-1 | KJ/m2 | 1.4 | ||
Rockwell hardness | ISO 2039-2 | — | 98 | ||
Electrical properties | Surface resistivity | IEC 60093 | Ω | >1016 | |
Volume resistance coefficient | IEC 60093 | Ω cm | >1014 | ||
Dielectric resistance coefficient | IEC 60167 | Ω | >1015 | ||
Dielectric strength | IEC 60243-1 | Kv/mm | 20 | ||
Dielectric constant | IEC 60250 | — | 3.5 | ||
Other properties | proportion | ISO 1183 | — | 1.19 | |
Molding shrinkage | ISO 294-4 | % | 0.2-0.6 | ||
Water absorption | ISO 62 | % | 0.3 | ||
Flame retardancy | UL94 | — | HB | ||