Share on (1601164545247):

Model | Density (Kg/m3) | Thickness (mm) | Width (mm) | Length (mm) | Thermal conductivity (W/m·K) |
GWR10 | 10 | 50 | 1200 | 30000 | 0.044 |
75 | 1200 | 20000 | |||
100 | 1200 | 15000 | |||
GWR12 | 12 | 40 | 1200 | 30000 | 0.042 |
50 | 1200 | 30000 | |||
75 | 1200 | 20000 | |||
100 | 1200 | 15000 | |||
GWR16 | 16 | 25 | 1200 | 30000 | 0.039 |
50 | 1200 | 15000 | |||
75 | 1200 | 10000 | |||
100 | 1200 | 7500 | |||
GWR24 | 24 | 25 | 1200 | 20000 | 0.036 |
50 | 1200 | 10000 | |||
75 | 1200 | 10000 | |||
100 | 1200 | 5000 | |||
GWR32 | 32 | 25 | 1200 | 20000 | 0.035 |
50 | 1200 | 10000 | |||
75 | 1200 | 10000 | |||
100 | 1200 | 5000 | |||
GWR48 | 48 | 25 | 1200 | 20000 | 0.032 |
50 | 1200 | 10000 | |||
75 | 1200 | 5000 | |||
100 | 1200 | 5000 |






Property | Test Method | Specification | ||
Temperature range | ASTM C411 | Up to 233 oC (450 oF) | ||
Moisture absorption | ASTM C1104 | < 1.0% at 49 oC, 95% RH | ||
Corrosivity | ASTM C665 | Does not accelerate | ||
Mold resistance | ASTM C665 | No growth | ||
Surface burning Characteristics Fire Test | ASTM E84 BS 476 Part 6,7 AS 1530-3 | Flame spread < 25 Smoke developed < 50 Class 0 Ignitability Index 0 Spread of Flame Index 0 Heat Evolved Index 0 Smoke Developed Index 1 | ||