Material | PAN- based Chopped carbon fiber |
Application | Electric Conductivity |
Carbon Content | >99.8% |
Thickness | 1.6-8 mm |
Width | 1.3-1.5 m |
Density | 0.09-0.12 g/cm3 |
Ash Content | <0.04% |
Resistivity | 0.0269-0.03Ω.m |
Tensile strength(longitudina) | 0.09-0.12 N/mm2 |
Tensile strength(transverse) | 0.06-0.07N/mm2 |
Elongation at break (longitudina) | 4%-6.5% |
Elongation at break (transverse) | 11%-18% |
Sulfur content | <0.001% |
Iron content | <0.02% |
Absorptivity | 17g/g |
Slagging rate | <0.2% |
BET | 2.7-4.4 m2/g |