Stainless Steel Welding Electrode/Welding Rod AWS 316L 16 E308L 16

Share on (60195840664):


Price:

Quantity:


Product Overview

Description


 

 

Company Information

We are factory!

 Shijiazhuang Shuanglu Machinery Co., Ltd.("Shuanglu" and "SUNLU" for short), as a member of China Welding Association (CWA) and one of the appointed manufacturers of China National Electric Equipment Corporation (CNEEC), manufactures complete welding electrode product.

Packaging & Shipping

Packing:

 2.5mm:2.5kg/box, 20kg/box, 2tons/pallet.

3.2mm:5kg/box, 20kg/box, 2 tons/pallet.

4.0mm:5kg/box, 20kg/box, 2 tons/pallet.

5.0mm:5kg/box, 20kg/box, 2 tons/pallet.

Or Custom !

 

Model

 Our factory supply:

 

AWS E6013,E7018,E7016,E6011, E6010,E308L-16,E316L-16,E308 welding electrode and mig wire!

 

Market

Market:

So far exported to Japan, Saudi Arabia,Qatar,USA, Brazil,  Ukraine,Thailand,Philipines,India,Pkistan,etc.

 

 

Product Description

Introduction:

 

E308L-16 is a kind of ultra-low-carbon Cr18Ni12Mo2 stainless steel electrode with lime-titania type coating. The carbon content of the deposited metal is lower than or equal to 0.04%. It has excellent heat-resistance, corrosion-resistance, crack-resistance, blowhole-resistance and welding performance. The coating has red-resistance and high strength. AC/DC.

 

Usage: 

 

Used for welding equipment of urea, synthetic fiber, etc. and stainless steel structures of the same types, and also used for Cr stainless steel which does not need heat treatment after welding, composite steel, dissimilar steel, etc.

 

Chemical Composition of Deposited Metal (%)

Chemical Composition

C

Mn

Si

S

P

Ni

Mo

Cr

Guarantee Value

≤0.04

0.5~2.5

≤0.90

≤0.020

≤0.030

11.0~14.0

≤0.75

17.0~20.0


Mechanical Properties of Deposited Metal

Test Item

Rm(MPa)

A(%)

-196℃ KV2(J)

Guarantee Value

≥490

≥30

≥32


Reference Current
(AC, DC+)

Electrode Diameter(mm)

φ2.0

φ2.5

φ3.2

φ4.0

φ5.0

Welding Current (A)

25~50

50~80

80~110

130~160

160~200


Instructions:
1.The electrodes should be baked under 250-300
for an hour before welding.
2.Direct current had better be used and the current should not be too strong.

 

    More detailed and photos, please be free to contact !