Polymer Modified Mortar For Styrofoam Coating

Share on (60382226212):


Price:

Quantity:


Product Overview

Description


Polymer Modified Mortar For Styrofoam Coating


Introduction :


This product is imported flexible polymer powder as the main additive , with high-quality materials and fine inorganic cementitious aggregate refining. Has excellent adhesion, breathability and crack resistance, and has some additional water features. This product is non-toxic, tasteless green products . Widely used in the insulation system on the base of thin plaster EPS polystyrene board , GRC board, pottery sticky boards and cement boards , etc., can be used with alkali-resistant glass fiber mesh used.


Application :
A:Suitable for inside and external plastering construction of aerated concrete blocks, sand-lime brick, ceramic tiles and other types of strong absorbent wall materials .
B:Suitable for inside and external plastering construction of clay brick, concrete hollow blocks , red wall tiles and other machines .
C:Reinforced concrete shear walls , plastering construction beams, columns, plates .
D:As surface mortar used in the EPS board , XPS insulation board , insulation mortar and other insulation material surface paving fiberglass mesh or steel mesh and leveling layer of primer .
E:This product is mainly used for commercial residential and industrial building's exterior wall or the insulation level of EPS / XPS insulation level special plaster cracking mortar .


Feature:


A:Wipe the surface layer does not bear the load .



B:Wipe the surface layer and the base layer have sufficient bond strength to make it in the construction or long-term environmental effects and no weight loss, no cracking .



C:Wipe the surface layer is thin and layered painting , the surface layer should be smooth , clean, beautiful and meticulous Lee .



D:Dry environment used for a large area exposed to the air .


 


Technical Date:


 




















































Test Program



Performance indicators



Tensile bond strength Mpa ( with cement mortar )



Normal condition 



≥0.70



temperature resistance



≥0.05



Water resistant



≥0.05



Freeze-thaw resistance



≥0.05



Tensile bond strength Mpa (with 181kg/m2 polystyrene board )



Normal condition 



≥ 0.10 and the destruction of polystyrene board



Water resistant



≥ 0.10 and the destruction of polystyrene board



Freeze-thaw resistance



≥ 0.10 and the destruction of polystyrene board



Operating time,h



1.5-4.0



Anti- crack



Thickness of 5mm or less free of cracks



Flexibility compressive / flexural strength



≤3.0



 


Picturer:


2_555_56850_400_400.jpg20107155782934076.jpg


ConcreteSelf leveling concrete


 


4.9214 s.