Introduction:


Cement pavement ( bridge ) repair materials specifically for cement concrete pavement ( bridge ) the pockmarked face , hollowing , peeling , sand , shell , crack, exposed tendons , peel , freeze-thaw exposed stones and other diseases for timely repair , can be directly applied to the site of disease ,
it has superior compressive strength and adhesion , enabling ultra-thin patch , and will not be broken off phenomenon at high pressure and high speed driving state ; all concrete surfaces are suitable for disease this material .


Feature:
A:Professional repair cement road pockmarked face , hollowing , peeling, shelling , cracks, exposed tendons , peel , freeze-thaw exposed stones and other diseases .
B:Pavement repair two hours after opening .
C:2mm thin repair can be achieved , not falling, not broken , tight seam .
D:2 hours compressive strength of up 42MPA, the highest intensity of 80MPA above .


Repair eight surface problem:


 A1.jpgA2.jpg


Product Performance:
a):Practical performance


No complicated construction machinery and technical requirements for the construction , no long closed to traffic , four hours after construction can open traffic ; without excavation site of the disease , can save a lot of construction costs, material costs and maintenance time , effectively delay the road diffusion and spread of the disease and prolong the service life of the road ; and after patching cement concrete pavement close to the original color , better aesthetics .
b):Bonding properties
The use of the material itself and the surface energy bonding capacity principle , with the original concrete surface repair reaction into a unified whole, thereby forming a high adhesive strength , the construction site of the disease with a variety of bonding, bonding capacity is not substantially affect the thickness can be realized 2mm thin patch in stretching , rolling , and other external forces and not fall off the passage , not broken .
c):Durability
Faster performance reflects the early and high early strength and late does not decay , the site can be done for many diseases at once eradicated ; the material itself has a strong waterproof , corrosion and UV resistance , and its anti-aging ability is original 5 times more cement concrete , performance degradation will not be earlier than the original concrete will not be lost due to aging bonding capacity and compressive strength.
d):Compression performance
After curing repair materials have a very strong compressive and flexural capacity , four-hour compressive strength of up to 42Mpa, 50Mpa strength can reach more than one day , late strength rising peak compressive strength of 80Mpa above , there are parts of the disease good reinforcing and supporting role , repair 3mm thickness can be achieved by non- road compression load requirements of special , high-speed and high-pressure driving status and will not be broken off .


Application:Airport runways, highway, road, municipal, tunnels, bridges, general concrete floor.etc.


Technical Date:


























































Test items



Unit



Technical Date



Test result



Setting time



Initial setting



min



≥5



8



Final setting



≤20



15



Compressive strength



30min



MPA



≥20



32



1d



≥30



53



28d



≥50



85



Drawing strength



28d



≥2.0



2.8



Expansion rate



28d



/



0.00%-0.1%



0.02%



Mixed with water available time



≥60min



  Construction steps:


 1.png2.jpg3.jpg4.jpg


Case Display:


 A):Highway pavement repair


B):Pavement repair Village Road


C): Parking lot pavement repair


 1.jpg2.jpg


Work Shop :


Indonesia Repair Mortar


 _.png


Business Card:


 


 Ryan Guo.png


0.2002 s.