Share on (60696104988):
| Material Property | ||||
| Hardness | 70 | Shore A | ||
| Tensile Strength | 12 | Mpa | ||
| Elongation at break | 320 | % | ||
| Hot air aging:100℃@168h | ||||
| Haedness changing | +2.1 | Shore A | ||
| Tensile Strength changing | +12 | % | ||
| Elongation at extension changing | -25.5 | % | ||
| Weight loss on heating | +2.5 | % | ||
| Hardness changing | ||||
| -20℃-0℃ | +2 | % | ||
| 0℃-23℃ | +1.5 | % | ||
| 23℃-70℃ | +2 | % | ||
| Th-40℃ | ||||
| Th-40℃ | No crack | / | ||
| Rubber parts appearance | ||||
| Appearance should be smooth, no distortion, no crack surface, no bubbles, no obvious impurities and other defects, color uniform | ||||
| Other properties | ||||
| Compression Set: 70℃@22h in 2mm | 57 | % | ||
| Heat shrinkage: 70℃@24h | 1 | % | ||
| ozone aging resistance 500pphm@Elongation 20%, 40℃168h | No Crack | / | ||