Share on (60711570915):
Item | Standard Values | Testing Result |
Tensile strength,MPa | ≥1.0 | 1.2 |
Elongation at break,(%) | ≥300 | 367 |
lmperviousness(0.3MPa,30min) | lmperviousness | lmperviousness |
Solid content,(%c) | ≥65 | 65 |
Drying time Surface drying time,(h) Actual drying time,(h) | ≤4 ≤8 | <4 <8 |
The tensile strength retention rate aftertreatment Heattreated,(%) Alkali treated,(% Acid treated,(%) | ≥80 ≥60 ≥40 | 141 82 78 |
Fracture elongation after treatment Heattreated,(%) Alkali treated,(%) Acid treated,(%) | ≥200 ≥200 ≥200 | 306 463 475 |
Heatshrinkage Elongation,(%) shorten,(%) | ≤1.0 ≤1.0 | ---- 0.3 |