AZS 33# 36# 41# Fused Cast Refractory AZS Brick For Float Glass Table Furnace

Share on (60735223747):


Price:

Quantity:


Product Overview

Description


AZS 33# 36# 41# Fused Cast Refractory AZS Brick For Float Glass Table Furnace

Product Description

 Advantage:

1.AZS block has passed ISO 

2.erosion-resistance to glass metal 

3.low pollution

AZS1.jpg

Description:

Our company can produce serious specification fused cast 33#,36#,41#AZS block for glass furnace ,and its output is over 5000tons per year. In the enormous working premises—more than 6600square meters, there are one 5tons outside cooling electric arc furnace, high-power transformer, thaw craft with computer control system and internal advanced fused cast refractory umeral caontrol grinding equipments according to its body producing ability.erosion-resistance to glass metal.

 Application:

Fused Cast AZS are the most widely used materials both in glass contact and superstructure of glass melting furnaces.

Fused Cast AZS 33% ZrO2: The reference category of fused-cast industry. Main applications include glass contact (paving tiles, working-end walls) and superstructures.

AZS2.jpg

Physical and chemical index

Item

Behaviors

AZS-33#

 

AZS-36#

 

AZS-41#

 

Chemical

Composition

Al2O3

≥50.00

≥49.00

≥45.00

ZrO2

≥32.50

≥35.50

≥40.50

SiO2

≤15.50

≤13.50

≤13.00

Na2O+K2O

≤1.30

≤1.35

≤1.30

Bulk density g/cm3

≥3.75

≥3.85

≥4.00

Apparent Porosity %

≤1.2

     ≤1.0

≤1.2

Cold Crushing Strength  Mpa

≥300

≥300

≥300

Exudation Temperature of Glass Phase

≥1400

≥1400

≥1410

Bubble Separation Ratio(1300°C×10h)

≤1.2

≤1.0

≤1.0

Anti-corrosion rate of glass liquid

1500°C×36h (mm/24h)%

≤1.4

≤1.3

≤1.2

Apparent density

(g/cm3)

PT(RN RC N)

≥3.50

≥3.50

≥3.70

ZWS(RR EVF EC ENC)

≥3.65

≥3.70

≥3.90

WS( RT VF EPIC FVP DCL)

≥3.75

≥3.8

≥4.00

AZS3.jpg

Packaging & Shipping

AZS4.jpg

Exhibition

AZS5.jpg