Share on (60760539376):
polyolefin heat shrink electrical pe cable insulation breakout boot
| Property | Test procedureand condition | TypicalPerformance | Test Method | |
| Physical | Water Absorption (%) | - | ≤0.15 | GB1034-1998 |
| Radial change (%) | 150±2°C/1~3min | ≥50 | - | |
| Longitudinal change, (%) | 150±2°C/1~3min | ≤10 | - | |
| Mechanical | Shore Hardness,A | - | ≤70 | GB2411-1980 |
| Tensile Strength, MPa (Mpa) | - | ≥14.0 | GB/T1040-1992 | |
| Ultimate elongation (%) | - | ≥500 | GB/T1040-1992 | |
| Cold bend | -55±2°C/1hr | No cracking | UL224-1992 | |
| Heat Shock | 250±1°C/4hr | No cracking | UL224-1992 | |
| After aging | Tensile Strength (Mpa) | 175±1°C/168hr | ≥70% | GB/T7141-1992 |
| Ultimate elongation (%) | 175±1°C/168hr | ≥70% | GB/T7141-1992 | |
| Electrical | Dielectric Strength (KV/mm) | - | ≥20 | GB1408-1989 |
| Volume Resistivity (Ω.cm) | - | ≥1.0×1013 | GB1410-1989 | |
| Dielectric constant | - | ≤3.5 | GB1409-1988 | |
| Chemical | Shrink temperature (°C) | - | 150 | - |
| flammability (OI) | - | ≥28.0 | GB/T2406-1993 | |







FAQ
Q 1: What is your quality warranty terms?
A: We will remake for free if you find some quality problems when you receive the products.
Q2: What’s the payment terms?
A: Generally. It’s T/T or L/C at sight for bulk order, also we accept the Western union or Money or Money gram or Paypal etc for small or sample order.
Q3: What’s your lead time?
A: For bulk order takes about 15-30days, for samples, take 3-5 working days.
Q4: Can you print on the products?
A: We can supply the print on the products as your demands.
Q 5: Can you help us to make the design?
A: OK, but please send us the logos or any contents you want to show.
New products from manufacturers at wholesale prices