I. composition characteristics and uses Our high-performance decorative acrylic electrophoretic coating is prepared by special process modification of acrylic monomer. Its strong resistance to salt fog, corrosion resistance, artificial sweat resistance, easy to operate and maintain performance, can be widely used in imitation gold jewelry, high-grade eyeglasses, door and window handle, lighting, box buckle, sanitary ware, kitchen utensils and other light industry products film application.
2. Technical parameters and performance standards 1Original lacquer property
2 Process parameters
3 Film technical index
3 Direction for use (1) Transpare e Electrophoretic bath Tank ratio electrophoretic primer: deionized water 1: 6-7 Methods: the original paint is placed in a barrel. In the case of no stirring, 2 to 3 times the deionized water is poured directly into the original paint, and then the clean mixing rod is stirred by hand or mechanical agitation to be completely dissolved (the general stirring time is 10-30 minutes), which can be added into the electrophoretic tank, filled with 6 to 7 times deionized. Water can open the electrophoresis tank circulating pump to circulate it for more than 12 hours. (2) Color electrophoretic bath Tank ratio electrophoretic primer: deionized water 1: 6-7 If a special water-soluble color paste is used for cathodic electrophoretic coating, then the color paste and deionized water can be manually stirred for 1-2 minutes at 1:3 ratio and then added to the pre-mentioned transparent electrophoretic bath solution, and the electrophoretic can be carried out after the circulation is sufficient. If oily color dye is used, it is divided into two steps: Step 1: put the original paint in a barrel and stir until the agitator or mixing rod and the wall of the barrel are covered with electrophoretic paint. Add the color paste to the original paint and mix well with the mixer or manual. Use a blender to ensure that the paint is not stirred hot (not too hot) Step 2: when stirring is stopped, add 2-3 times of water to the original lacquer, add electrophoretic tank evenly by hand or mechanical stirring, add deionized water with 6 to 7 times of original paint, then open the electrophoretic tank for 12 hours to add film to electrophoretic electrophoresis. 3. Method of adding lacquer First, put the added paint in a clean barrel, then 2-3 times the original slots of the need to fill the original slots, the manual mixing, and then pour into the electrophoretic tank for 0.5 hours (the principle of adding paint should follow the principle of a small number of many times). 4 Matters need attention 1 Pure water quality required below 10µs / cm 2 Tank liquid temperature should be controlled between 25 ℃ and 35 ℃ (heated in hot water bath or cooled by ice or cooler) 3 To clean the workpiece, do not bring acid and alkali into the tank. 4 Electrophoretic bath renewal or supplementation requires a circulation of more than 0.5-1 hours before the electrophoresis operation. 5 When adding excipients, the principle of "small amount and many times" should be taken as the principle, which is beneficial to the stability of bath liquid. 6 Follow the basic process parameters, regularly detect the solid content and pH, conductivity and adjust the solvent content in the bath solution. 7 In the case of low dosage and slow regeneration, appropriate amount of solvent should be added to the electrophoretic tank, and no solvent should be added to the fast-renewing tank, unless the electrophoretic cell, which is often required for ultrafiltration due to poor pretreatment and cleaning, needs to be supplemented with a proper amount of solvent.
Detailed Images
Packing & Delivery
Packaging:50KG/20KG/1000KG storage:Store in a cool, dry place,the storage period is six months.If it exceeds the storage period, it can still be used after the inspection is qualified