Share on (62298497307):
Manufacturer Brake Pads Price for Phenolic Resin



This series can efficiently control the roller hardening time with advanced processing, which characterized in good insulation, humidity and heat resistance, stability in size and excellent molding range, good wetting property with other fillings possessing in various polarities. It also can used in the rubber modification to increase the rubber intensity.
PF2123D series technical data:
Grade | Appearance | Softening point(℃) (International standard) | Pellet flow /125℃(mm) | Cure /150℃(s) | Application/ Characteristic |
2123D1 | Light yellow flakes or white flakes | 85-95 | 80-110 | 40-70 | Common |
2123D2 | 95-105 | 70-100 | 40-60 | ||
2123D3 | 85-100 | 60-100 | 40-60 | High intensity | |
2123D4 | 90-100 | 60-90 | 30-50 | High ortho, High intensity | |
2123D5 | Brown red sheet | 90-102 | 60-90 | 50-70 | Common |
Packing and storage:
Powder: 20 kg or 25 kg/bag, blocks,flakes: 25 kg/bag. Packed in woven bag, lined with plastic liner, or in kraft paper bag, lined with plastic liner. Resin should be stored in a cool, dry and well ventilated place far away from heat source to avoid moisture and caking. The storage life is 4-6 months below 20℃. Its color will become dark with the storage time, which will do no influence on the resin grade.