Основной чугун с низким содержанием серы и фосфора

Сохранить в закладки 10000003611478:


Цена:660,00 $*

Количество:

  • В избранное

Описание и отзывы

Характеристики



Product Description


Features of product


Pig iron is produced from the blast furnace. The purpose of a blast furnace is to chemically reduce and physically convert iron oxides into liquid iron called "hot metal". The blast furnace is a huge, steel stack lined with refractory brick, where iron ore, coke and limestone are dumped into the top, and preheated air is blown into the bottom. The raw materials require 6 to 8 hours to descend to the bottom of the furnace where they become the final product of liquid slag and liquid iron. These liquid products are drained from the furnace at regular intervals. The hot air that was blown into the bottom of the furnace ascends to the top in 6 to 8 seconds after going through numerous chemical reactions. Once a blast furnace is started it will continuously run for four to ten years with only short stops to perform planned maintenance.


Pig iron is an intermediate product and the first product of Ironmaking reduced from Iron ore. Pig iron has a very high carbon content, typically 3.5–4.5%,[1] along with silica, Manganese, Sculpture, Phosphorus, Titanium and other trace elements.


Uses and benefits of the product:


Pig Iron comprises three main types: BASIC PIG IRON, used mainly in electric arc steelmaking, FOUNDRY PIG IRON used mainly in the manufacture of grey iron castings in cupola furnaces, and NODULAR PIG IRON (SG GRADE) used in the manufacture of ductile iron castings. Pig iron is used for steel making, Foundries, Alloy making, in automotive castings and other iron-based castings.


 


 WIKI-10.jpg


 





Packaging & Shipping


We confirm packing as per the buyer arrange to ship


 





Our Services


Capability to meet huge market demands


·Safe & Hygienic Packaging


·On-time delivery schedule


·Competitive pricing policy


·Customer-centered approach


·Putting high business ethos in practice


 





Company Information

 

 
























Basic grade Pig Iron.
Chemical Composition :C:3.5-4.5%;Mn :0.4-1.0%;Si:0.5-1.2%;P:0.15% Max;S:0.04% Max



- Each pig weighing 45 kg. max,with two notches.
- Low sulphur and phosphorus content due to superior iron ore and low ash coke.



On a draft survey basis.



On an actual weight basis.



On mutually agreed terms.



- Test Certificate is issued on the basis of Cst Analysis.   Pig Iron is produced from a 3200 Cu.m blast furnace using Iron Ore from Bailadilla (One of the best ores in the world), low ash Coke (using a high percentage of imported Coal in the blend). A high Sinter percentage in the burden ensures low Sulphur and Phosphorus contention in the Pig Iron



Pig Iron




























































Grade



Carbon



Silicon



Manganese



Sulphur



Phosphorus



Basic Grade



3.5% - 4.6%



1.25% max



0.4% - 1.2%



0.07% max



0.14% max



Nodular/SG Grade



3.5% - 4.6%



1.25% max



0.3% max



0.015% max



0.08% max



3.5% - 4.6%



1.25% - 2.25%



0.3% max



0.015% max



0.08% max



Foundry Grade



3.5% - 4.3%



1.75% - 2.00%



1.00% max



0.07% max



0.14% max



3.5% - 4.3%



2.00% - 2.50%



1.00% max



0.06% max



0.14% max



Semi Foundry Grade



3.5% - 4.6%



1.25% - 1.75%



0.4% - 0.8%



0.07% max



0.10% max



 