Жидкий материал белый цвет RTV2 оловянный силиконовый каучук для изготовления полиуретана/смолы/ювелирных изделий

Сохранить в закладки 11000008094792:


Цена:*

Количество:

  • В избранное

Описание и отзывы

Характеристики



Product Description


Model Code
GTSIL-T10
GTSIL-T15
GTSIL-T20
GTSIL-T25
GTSIL-T30
GTSIL-T35
GTSIL-T40
Hardness-Shore A
8-10
14-16
19-21
24-26
28-32
34-36
38-40
Viscocity-Cps
10000-14000
12000-16000
14000-18000
16000-20000
26000-32000
33000-38000
10000-14000
Mixing Ratio - %
100:2, 100:3, 100:5
100:2, 100:3, 100:5
100:2, 100:3, 100:5
100:2, 100:3, 100:5
100:2, 100:3, 100:5
100:2, 100:3, 100:5
100:2, 100:3, 100:5
Tear strength - Kn/m2
10-15
15-18
19-23
23-27
25-30
25-28
16-20
Tensile strength - Mpa
3.5-5.5
3.5-5.5
4-6
4-6
5-7
5-7
3.5-5.5
Shrinkage - %
0.3%
0.3%
0.3%
0.3%
0.3%
0.3%
0.3%
Elongation - %
400-500%
400-500%
400-500%
400-500%
350-500%
350-500%
350-500%




Feature & Advantage


1. Low viscosity for easy mixing,great for making simple one- or two-piece block molds.
2. Perfect for art and industrial applications,often used for molds to reproduce sculptures and other prototypes, casting plaster, resins, and wax.
3. Very good fluidity for easy pouring operation.
4. Stable quality & non-oily.
5. Good tension for easy de-molding.
6. Good duplication with fine details.
7. High performance in replication.
8. Excellent resistance against heat, acid & alkali and aging.
9. Low shrinkage (around 0.2%).
10. Long Shelf-life up to 18months.





Packing & Delivery






Regular package: 1kg/drum, 5kg/drum, 20kg/drum, 25kg/drum, 200kg/drum
Customization package is available.

Shipment:
* Samples: 1-3 days with upon receipt of your payment
* Mass production order: normally 3-7 days after having your payment.
* For more detailed information, kindly ask me, thanks~!


Application








certification






Company Profile


Our strength:
1. Owning 5 factories located in Dongguan and Hengyang,Hunan (Sanpin, Sanqi, Huacan, Dongguang Gangtian, Hunan Gangtian)
2. Factory size above 50000 square meters in total.
3. In Hengyang, Hunan, we have an industrial park, around 25000 M2.
4. All relevant certificates are avaialble: FD*, MSDS, REACH, ROHS, Cargo safe transportation by Sea/Air.
6. 600 tons per month capacity so far, can enlarge anytime.
Welcome to visit our factory~!










Common Question and Our warm advice and solutions.

******Why could the silicone mold be reused only for a few times?
Maybe you will confuse about this question for years. Here we share you some following reasons:
* Adding too much silicone oil into silicone rubber. Silicone oil is an additive which will destroy the molecular weight of
silicone rubber and reduce the tension and tear strength.
* Adding too much catalyst into the silicone rubber when you make the molds. For the condensation cure(tin catalyst) silicone rubber. we s est you add no more than 2% of catalyst. If you 1add too much catalyst, the operation time will be too fast to operate ,which will also reduce the tension and tear strength.
* Using the silicon rubber with a high hardness to make molds for small sized products with delicate and intricate designs and the silicon rubber with a low hardness to makes molds for large sized products with simple designs.

******Why does the silicone mold get burnt out?

The silicone mold get burnt out because you have left out the important notes when using unsaturated resin materials to produce your products. The unsaturated resin produces great heat when added the curing agent. So you must demould the product within 3 minutes to avoid this problem.
Our silicone rubber has add a special material which can resistant high temperature to make the resin molds. Help our customer avoid this problem.

******Why does the silicone mould appear to be dry outside but wet inside?
Because molding silicone rubber is a kind of condensation silicone rubber, which get solidified after absorbing moisture from the air. In order to provide a significant shelf-life for the silicon rubber, we will dry out the water in the silicon rubber.
Solution: Add 0.05% water into the silicon rubber and Stir over a low speed briefly when you use it.

******Why is the tear strength of silicone molds weak?


There are three reasons:
1) In order to reduce the viscosity of silicone rubber and pursue good quality, a large amount of silicone oil can be added to the silicone rubber when making the mold. In fact, it may have the opposite effect. The addition of silicone oil can severely reduce tension and tear strength. And the silicon mold will be in a fragile and fragile state.
2) too much catalyst may be added to the silicone rubber, we recommend that customers add catalyst no more than 5%, 2% is fine.
3) After the silicone mold is finished, you may use it prematurely. We recommend that customers start using the mold after 24 hours. More importantly, it would be better if you could make an outer mold to protect the silicone mold.

******Why does the mold silicone have poor tension?

In the process of making the mold, in order to reduce the viscosity of the silicone rubber and make the silicone rubber easy to operate, a large amount of silicone oil is added to the silicone rubber, which will make the silicone rubber very soft, resulting in poor tensile strength and reduced tear strength. The phenomenon of poor tensile force, resulting in the phenomenon that the mold is not durable, the service life is short, and the number of mold overturns is small.

******Why does the mold appear oily?

The mold silicone itself will not emit oil. The oil is caused by the addition of composite silicone oil (complex of silicone oil
and white mineral oil) during the operation, because white mineral oil is a petrochemical product, not silicone oil.

******Why does the silicone mold have traces, streaks, and unevenness on the surface?

This phenomenon occurs because the product or model to be reproduced has not been ground or polished. Because the actual model or product itself is not smooth or perfect enough, if the product or model to be copied has not been ground or polished, even the best silicone mold will be unsightly and not smooth enough. Another situation is that when the release agent is applied, the mold will not be smooth if it is not evenly brushed.