Test item | Unit | Index |
Tensile strength | MPa | >=13.5 |
Rupture elongation | % | >=350 |
Impact brittle temperature | -76 | |
Impact brittle performance | Failure rate | <=15/30 |
Heating aging temperature | 135+-2 | |
Duration | H | 168 |
Tensile strength change rate | % | +-20 |
Rupture elongation change rate | % | +-20 |
Hot drawing | % | <=80 |
Keep permanent deformation after cooling | % | <=5 |
Gel contents | % | >=80 |
Dielectric loss factor | <=1X10-3 | |
Relative dielectric constant | <=2.35 | |
Volume resistivity | O.m | >=1X1014 |
Dielectric strength | MV/m | >=25 |