Бумажная пенопластовая доска
US $0.24-$0.26
Сохранить в закладки:
POM Certificate Of Quality | ||||||||||
Items | Test situation | Test method | Test data | Unit | ||||||
Basic property | Density | ASTM D792 | 1.42 | g/cm3 | ||||||
Water absorb | 24hrs soak +73℉(+23℃) | ASTM D570 | 0.25 | % | ||||||
Water absorb | Equi1.50%R.h.+73℉(+23℃) | ASTM D570 | 0.22 | % | ||||||
Water absorb | Soak F point +73℉(+23℃) | ASTM D570 | 0.9 | % | ||||||
Mechanical property | No notch impact strength | 23℃ | D256 | >5300 | j/m | |||||
Compression elasticity | 73°F@10%Def. | ASTM D695 | 18 | Mpsi | ||||||
Compression elasticity | 23℃@10%Def. | ASTM D695 | 124 | Mpa | ||||||
Deformation on load | 2000psi@+122□H(14Mpa@50℃) | ASTM D621 | 0.5 | % | ||||||
Curving surrenders strongly | 73℉ | ASTM D671 | 4.7 | Mpsi | ||||||
Curving surrenders strongly | 23℃ | ASTM D671 | 32.4 | Mpa | ||||||
lzod impact strength | 40℉ | ASTM D256 | 1.8 | ft.lb/in | ||||||
lzod impact strength | 40℃ | ASTM D256 | 96.1 | j/m | ||||||
lzod impact strength | 73℉ | ASTM D256 | 2.3 | ft.lb/in | ||||||
lzod impact strength | 23℃ | ASTM D256 | 123 | j/m | ||||||
Tensile impact resistance | 73℉ | D1822Long | 170 | ft.lb/in2 | ||||||
Tensile impact resistance | 23℃ | D1822Long | 350 | Kj/m | ||||||
No notch impact strength | 73℉ | ASTM D256 | >100 | ft.lb/in | ||||||
Tensile Strength rate | 68℉(-55℃) | ASTM D638 | 38 | % | ||||||
Tensile Strength rate | 73℉(+23℃) | ASTM D638 | 75 | % | ||||||
Tensile Strength rate | 158℉(+70℃) | ASTM D638 | 230 | % | ||||||
Tensile Strength rate | 212℉(+100℃) | ASTM D638 | >260 | % | ||||||
Tensile Strength rate | 250℉(+122℃) | ASTM D638 | >260 | % | ||||||
Elasticity range | 68℉ | ASTM D638 | 14.7 | Mpsi | ||||||
Elasticity range | 55℃ | ASTM D638 | 101 | Mpa | ||||||
Elasticity range | 73℉ | ASTM D638 | 10 | Mpsi | ||||||
Elasticity range | 158℉(+70℃) | ASTM D638 | 6.9 | Mpsi | ||||||
Elasticity range | 70℃ | ASTM D638 | 47.5 | Mpa | ||||||
Elasticity range | 212℉ | ASTM D638 | 5.2 | Mpsi | ||||||
Elasticity range | 100℃ | ASTM D638 | 35.9 | Mpa | ||||||
Elasticity range | 250℉ | ASTM D638 | 3.8 | Mpsi | ||||||
Elasticity range | 122℃ | ASTM D638 | 26.2 | Mpa | ||||||
Elasticity coefficient | 73℉ | ASTM D638 | 450 | Mpsi | ||||||
Elasticity coefficient | 23℃ | ASTM D638 | 3100 | Mpa | ||||||
Shearing force | 73℉ | ASTM D732 | 9.5 | Mpsi | ||||||
Shearing force | 23℃ | ASTM D732 | 65.5 | Mpa | ||||||
Winding coefficient | 68℉ | <25℃ | 530 | Mpsi | ||||||
Winding coefficient | 55℃ | <25℃ | 3650 | Mpa | ||||||
Winding coefficient | 73℉ | <25℃ | 380 | Mpsi | ||||||
Winding coefficient | 23℃ | <25℃ | 2620 | Mpa | ||||||
Winding coefficient | 158℉ | <25℃ | 225 | Mpsi | ||||||
Winding coefficient | 70℃ | <25℃ | 1550 | Mpa | ||||||
Winding coefficient | 212℉ | <25℃ | 130 | Mpsi | ||||||
Winding coefficient | 100℃ | <25℃ | 895 | Mpa | ||||||
Winding coefficient | 250℉ | <25℃ | 90 | Mpsi | ||||||
Winding coefficient | 122℃ | <25℃ | 620 | Mpa | ||||||
Curving surrenders strongly | ASTM D790 | 14.3 | Mpsi | |||||||
Curving surrenders strongly | 218℉ | ASTM D790 | 98.6 | Mpa | ||||||
Compression elasticity | ASTM D695 | 5.2 | Mpsi | |||||||
Compression elasticity | ASTM D695 | 35.9 | Mpa | |||||||
Tensile Strength | ASTM D-638 | 68.9 | Mpa | |||||||
Rockwell hardness | ASTM D785 | M94,R120 | ||||||||
Physical property | Insulation Strength | Short Time,90mils | ASTM D149 | 500 | V/mil | |||||
Insulation Strength | Short Time,2.3mm | ASTM D149 | 1.97 | MV/m | ||||||
Friction coefficient | +73℉(+23℃)Static | 0.20 | washertest3 | |||||||
Friction coefficient | +73℉(+23℃)Dynamic | ThrustWasher | 0.35 | |||||||
Resistance coefficient | +73℉(+23℃)0.2%H20 | ASTM D257 | 10 15 | Ohm-cm | ||||||
Insulation Strength | Coefficient+73℉(+23℃)102to106Hz | ASTM D150 | 3.7 | |||||||
Diffusion factor | +73℉(+23℃)10^6Hz | ASTM D150 | 0.005 | |||||||
Electricity property | Arc resistivity | 120mil(3.1mm) | ASTM D495 | 220no tracking | sec | |||||
Hot deformation temperature | 0.5Mpa | ASTM D648 | 172 | ℃ | ||||||
Hot deformation temperature | 1.8Mpa | ASTM D648 | 136 | ℃ | ||||||
Hot deformation temperature | 66psi | ASTM D648 | 342 | ℉ | ||||||
Hot deformation temperature | 264psi | ASTM D648 | 277 | ℉ | ||||||
Melting point | ASTM D2133 | 347 | ℉ | |||||||
Melting point | ASTM D2133 | 175 | ℃ | |||||||
linear thermal expansion coefficient | -40to+85℉ | ASTM D696 | 5.8 | 10-5in/in.℉ | ||||||
linear thermal expansion coefficient | -40to+85℉ | ASTM D696 | 10.4 | 10-5m/m℃ | ||||||
linear thermal expansion coefficient | -85to+140℉ | ASTM D696 | 6.8 | 10-5in/in.℉ | ||||||
linear thermal expansion coefficient | -29to+60℃ | ASTM D696 | 12.2 | 10-5m/m℃ | ||||||
linear thermal expansion coefficient | -140to+122℉ | ASTM D696 | 7.6 | 10-5in/in.℉ |