Share on:
Ni | 52-60 | Cr | 14.5-16.5 | Fe | 4-7 |
Mo | 15-17 | P | ≤0.04 | Mn | ≤1 |
S | ≤0.03 | C | ≤0.02 | Si | ≤0.08 |
density g/cm3 | Melting point ℃ | Thermal conductivity λ/(W/m•℃) | Specific heat capacity J/kg•℃ | Elastic Modulus GPa | Resistivity μΩ•m | Linear expansion coefficient a/10-6℃-1 |
8.9 | 1325-1370 | 10.2(100℃) | 407 | 208 | 1.25 | 11.7(100℃) |
Heat treatment method | Tensile strength σb/MPa | Yield Strength σp0.2/MPa | Elongation σ5 /% |
Solution treatment | 690 | 283 | 40 |
Alloy grade | Form | Specification | ||
Hastelloy C276 | Wire | Diameter=0.025mm~8mm | ||
Hastelloy C276 | Flat wire | Width=0.4~40mm | Thick=0.03~2.9mm | |
Hastelloy C276 | Strip | width=8~250mm | ThickT=0.1~3.0mm | |
Hastelloy C276 | Foil | width=6~120mm | Thick=0.003~0.1mm | |
Hastelloy C276 | Bar | Diameter=8~100mm | Long=50~1000 |