To better ensure the safety of your goods, professional, environmentally friendly, convenient and efficient packaging services will be provided.
Company Profile
Procedure Content (1)Dilution and viscosity adjustment To stir for 5-10 minutes till it’s well proportioned. If the viscosity needs to be adjusted, 1-2% of the diluent can be added in. It’s recommended to use BCS diluent.
(2)Standing To stand 10-15 minutes after fully stirring, and then to process screen printing. (3) Screen mesh Either 36T or 43T is available
(4)Pre-curing A:To print and cure each side separately: The first side in hot air circulating oven: 75±5℃、15-20 minutes. The second side in hot air circulating oven: 75±5℃、20-25 minutes. B:To print and cure two sides at the same time. Hot air circulating oven: 75±5℃、25-35 minutes.
(6) Developing Developing solution: (1±0.2%) of Na2CO3 solution Temperature of developing solution: 30±2℃ Developing time: 40-60 seconds Washing pressure: 1.8~2.2kg/c㎡ (7)Posterior curing Temperature: 150±5℃ Curing time: 60 minutes Matters need attention: 1. To fully stir till it’s well-proportioned before using it. 2. Parameters above is only for reference, the specific operation should be subject to samples.